MODELIS

G.W

IZMĒRS (mm)

A

Bmin

C

D

E

F

G

Hmin

EPC13

2.5

13.3±0.3

8.3

5.6±0.2

4.6±0.2

4.5±0.2

6.6±0.2

2.1±0.1

10.5

EPC17.8

5.6

17.8±0.4

11.5

7.4±0.2

6.0±0.2

6.0±0.2

8.7±0.2

2.8±0.1

14.3

EPC34

62

34.0±0.5

19.7

14.5±0.2

14.5±0.2

16.4±0.2

20.9±0.2

9.1±0.2

24.8

EPC39

78

39.0±0.7

24.7

17.6±0.3

15.5±0.2

14.1±0.3

19.6±0.2

9.7±0.1

30.5

EPC41

108

41.0±0.6

23.6

18.5±0.2

16.5±0.2

18.9±0.2

24.5±0.2

11.0±0.2

28.8

 

MODELIS

PARAMETRS

AL±25% (nH/N^2)

N.W(g)

C1mm-1

Lemm

Aemm2

Vemm3

ZP40

EPC13

2.46

30.6

12.5

382.0

870

2.1

EPC17.8

1.77

40.2

22.7

917.0

1200

4.5

EPC34

0.73

89.6

122.6

10985.0

3200

56.0

EPC39

0.60

87.95

147.0

12960.0

3700

70.5

EPC41

0.57

104.1

183.2

19064.0

4100

97.0